Photonics & AILU
Design for Laser Manufacture - Inspiring designers to 'think laser'

Back to

Laser coated steel pipe

Copyright of ©2006 Fraunhofer Institute IWS Dresden
Copyright of ©2006 Fraunhofer Institute IWS Dresden
Copyright of ©2006 Fraunhofer Institute IWS Dresden

Cold work steel 90MnCrV8 (O2) crack-free coated with NiCrBSi alloy Deloro 60. More details can be found in the document ‘Induction assisted laser materials processing’ [link here].



 

View Picture (299kB)

Copyright of ©2006 Fraunhofer Institute IWS Dresden
We make every effort to trace copyright. If inadvertently we have not attributed copyright or attributed it incorrectly, please contact us using our webform or by emailing dlm@ailu.org.uk and we will rectify the situation.

Disclaimer

To view disclaimer details click here